Sunday, August 23, 2009

[MW:2994] RE: 2992] Re: LTCS Consumables

[MW:2992] Re: LTCS Consumables
Dear all,
A333 Gr6 (LTCS) calls for impact testing requirement.
E6010 root will not give impact strength. You need to go for ER70 S2 (spl) for root with E7018-1 for fill up and capping.
 
Regards,
 
R.Gopalasamy,
Sr.QA/QC Consultant,
Hindustan Oil Exploration Company Ltd,


-------------------------------------------------------------------- HOEC Email Disclaimer : http://www.hoec.com/email_disclaimer.htm



From: materials-welding@googlegroups.com on behalf of Amarjit Singh
Sent: Sat 8/22/2009 1:44 PM
To: Materials & Welding
Subject: [MW:2992] Re: LTCS Consumables


dear,
E-7018-1 is suitable for charpy impact upto -45 deg C U can qaulify
iwith E7018-1
Amarjit singh

On Jul 22, 10:01 am, "Nikhil" <nikhilrp_2...@rediffmail.com> wrote:
> Dear Friends,
>
> I like to know whether we can use the combination of E6010 in root and E7018-1 as filler in LTCS (A333Gr6) welding, particularly in Ammonia service (flash point is minus 33 deg C)?
>
> The working temp is less than minus 33 deg C. At what temp should I impact test it?
>
> Regards,
>
> Nikhil
> QC Engineer
> Sharjah, UAE
> +97150 1453525
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...