[MW:2203] Re: coating thicknesss on rcc structures

ultrasonic measuring gauges are available. pl refer the attchement for one such model

 
On Mon, May 18, 2009 at 2:10 PM, kevin mathew <kmvkeralaa@yahoo.co.in> wrote:
please gave me confirmation how we can check DFT ON RCC or concrete structures
 
kevin


Explore and discover exciting holidays and getaways with Yahoo! India Travel Click here! --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

2 comments:

Unknown said...

Kevin, where is the attachment?


Thanks
Senthil

BR said...

you can check on group's home page.

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...