Wednesday, December 24, 2008

[MW:1416] Re: welding reqd on a weldolet

I would advise you to refer ASME Sect VIII Div 1 UW-16.After filling the groove,the fillet size(Leg length) need not exceed 3/4".
Regards
Aarpee

On Wed, Dec 24, 2008 at 6:23 AM, Vinod Upadhyay <vinod.vru@gmail.com> wrote:
Pls find the attached table showing groove and fillet requirements of Weldolets.
May be helpful to u.

Regards

Vinod


On Tue, Dec 23, 2008 at 5:39 PM, HAREESH K V <hareesh13h@gmail.com> wrote:
Dear Sir,

Please find herewith the welding we have done on a weldolet as per
client requirement.

Is this much welding required?

Please share your views.

--
Hareesh K V










--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...