Interpass temeprature is measured between complete of one pass and before start of next pass and normally the interpass temperature shall be maintained between min specified preheat and max limits of interpass .Whenever low interpasses are required it is better to allow more time lapse between the passes and we normally do not measure the temperature of the bead during welding and I hope it is not specified any where in the codes.

To control colour tint may be other parameters also looked into.such as trailing gas flow etc to keep the wled zone free of any oxidation and also it provides the cooling effect also thereby the colour tint may be reduced .


Best Regards,

Francis Lobo
----- Original Message -----

From: claes gillenius

To: materials-welding@googlegroups.com

Sent: Mon, 15 Dec 2008 22:39:51 +0530 (IST)

Subject: [MW:1404] Re: Interpass temperature measurement.






When we test electrodes / weld metal

properties / here, we interpret interpass temp. as the max. temp. when

a new pass can be started. We do continue with the next electrode directly

after the first regardless of temp. I.e. we measure interpass temp before

starting the next weld bead. However, we do not weld titanium, so I understand

there may be a problem in that case.












Claes Gillenius


Development Engineer, MMA. (Spec. stainless and non Fe-alloys)


Direct tel:  +46 (0)31 509315


Mobile +46 (0)707532012


Company                ESAB

AB


Address                

 Box 8004, 402 77  Gothenburg, Sweden


               

                 Lindholmsallén

9


Company  reg number        556005-7738

















kataiah@bilfal.com




Sent by: materials-welding@googlegroups.com

2008-12-15 04:06







Please respond to


materials-welding@googlegroups.com

















To


materials-welding@googlegroups.com



cc






Subject


[MW:1401] Interpass temperature measurement.


























Dear Friends,


I have a confusion regarding the measurement of interpass

temperature.During GTAW welding of Titanium material, interpass temperature

should be maintained very low to avoid oxidation (Blue color formation).

When weld length is more, the moment welder starts welding   interpass

temperature exceeds the specified limit. Before welding with next rod,

interpass temp will be higher than specified but generally  we won't

stop welding until total run or weld length is completed.


 


Please advise me when to measure interpass temperature.  


Regards


 


P.K  














This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it. ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.



--
KLUB MJ Hunt, Search for India's First Movie Jockey
For more details log on to http://www.zeecinema.com
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS