[MW:1393] Re: CVN Impact exemption on PQR as per UCS 67 (a) (2)

CVN impact is required on PQR as per my opinion.Data given in mfr's data sheet can not be recognised.It can ofcourse increase our confidence after using and subsequent testing at MDMT in question.
Regards
Aarpee

On Tue, Dec 9, 2008 at 3:54 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

MDMT -46 °C

MOC: SA333 Gr6, SA 350 LF2, cl1, both are exempted from CVN impact as per UCS 66(g)

Consumables used are ER80SNi-1, and E7018 G as per SFA5.5 (both are tested at -60 °C with satisfactory values as per mfr data sheet)

However PQR impact testing required unless consumable are classified by impact tests at least at -46 °C by the applicable SFA as per UCS 67 (a) (2).

In this case E 7018-G (ETC PH 76S of Oerlikon) as per SFA 5.5 does not satisfy this rule.

In my opinion CVN impacts are required on PQR. Members please share your opinion/interpretation.





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...