When Impact test is Applicable, according to ASME Sec.IX, change in AWS classification is an supplementary essential variable and cannot be changed.. Thanks & Regards J.Gerald Jayakumar 0091-8838619635 On Saturday, 10 October 2026 at 07:36:48 pm IST, Noble <noblejohny94@gmail.com> wrote: Dear Experts, If a PQR is qualified using ER70S-2 with impact testing, can we use the same PQR to prepare a WPS using ER70S-6, since both filler metals fall under the same F-Number and A-Number? Would this be acceptable under ASME Section IX, or would a new PQR be required? Your expert opinions and code references would be appreciated. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Material...
Materials selection, welding, forming, Heat treatment, corrossion, NDT