Dear Mohammed, Thank you for your response. We're facing another significant issue. Most of our carbon steel Procedure Qualification Records covering groups G1-G2, G1-G3 & G2-G3, G3-G3 with various process combinations are showing an unacceptable hardness range (260–325 HV) in the Heat-Affected Zone. Our maximum acceptable hardness limit is 250 HV. We've used different testing agencies, yet the results remain consistently high. Regards, Saurabh On Fri, 17 Oct 2025 at 8:26 AM, Mohmmed Dudhiyawala < mdudhiya007@gmail.com > wrote: Dear Saurabh, Refer Table A.12 of NACE MR0175/ISO 15156, where Inconel 625 is designated as Type 4d. Refer Table A.14. From Temp<149°C, Inconel 625 can be used for all conditions, stipulated in table. Hardness to be limited to 40 HRC max. (392 HV). Regards, Mohammed On Tuesday, August 19, 2025 at 7:47:46 AM UTC+5:30 Saurabh Jain wrote: Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. ...