Re: [MW:32757] impact test difference in WPS & MTC

Welding consumables do not mandatorily require test certificates.  Manufacturer's certification on the packaging is acceptable as per the Code.  Consumable once certified by manufacturer for a certain classification is understandable he has made all the necessary tests including impact testing and these consumables can be used upto the lower temperature as per the mentioned classification. If you are using the consumable at lower temperature than classified according to the consumable specification it is necessary to have a Batch test certificate from the manufacturer.  If not run a production test coupon and perform Impact test only. Regards,   Prashant P Rane On Mon, Jan 17, 2022 at 1:32 PM 'sangram routray' via Materials & Welding < materials-welding@googlegroups.com > wrote: Dear Experts, we have a qualified PQR & WPS with impact test @ -52°C , with use a specific filler wire batch.  In witch filler wire MTC; manufacture recommended the impact val...

Re: [MW:32756] impact test difference in WPS & MTC

NO the specific batch test not yet as per ASME Sec-II part C. only WPS qualified on -52°C  Thanks & Regards Sangramkeshari Routaray MOB NO. +91-8249921885 On Monday, 17 January, 2022, 03:22:55 pm IST, Vishwas Keskar <vvkeskar123@gmail.com> wrote: Is this specific batch is tested and certified as per ASME.SEC II  Part C for Impact testing at - 52 Deg C ? On Mon, 17 Jan 2022, 15:02 'sangram routray' via Materials & Welding, < materials-welding@googlegroups.com > wrote: Dear Experts, we have a qualified PQR & WPS with impact test @ -52°C , with use a specific filler wire batch.  In witch filler wire MTC; manufacture recommended the impact value @ -40 °C. Job's Impact requirement is -52°C. shall I use the same specific batch Filler wire for the job?? (Y/N) or required ba...

Re: [MW:32755] impact test difference in WPS & MTC

Is this specific batch is tested and certified as per ASME.SEC II  Part C for Impact testing at - 52 Deg C ? On Mon, 17 Jan 2022, 15:02 'sangram routray' via Materials & Welding, < materials-welding@googlegroups.com > wrote: Dear Experts, we have a qualified PQR & WPS with impact test @ -52°C , with use a specific filler wire batch.  In witch filler wire MTC; manufacture recommended the impact value @ -40 °C. Job's Impact requirement is -52°C. shall I use the same specific batch Filler wire for the job?? (Y/N) or required batch test qualification (all weld test ) Answer with code's justification.   welding code ASME Sec-IX code of construction ASME B31.3 Thanks & Regards Sangramkeshari Routaray MOB NO. +91-8249921885 -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To...

[MW:32753] impact test difference in WPS & MTC

Dear Experts, we have a qualified PQR & WPS with impact test @ -52°C , with use a specific filler wire batch.  In witch filler wire MTC; manufacture recommended the impact value @ -40 °C. Job's Impact requirement is -52°C. shall I use the same specific batch Filler wire for the job?? (Y/N) or required batch test qualification (all weld test ) Answer with code's justification.   welding code ASME Sec-IX code of construction ASME B31.3 Thanks & Regards Sangramkeshari Routaray MOB NO. +91-8249921885

Re: [MW:32753] Selection of Pigs For 30" Gas Pipeline

For pigging you need min 5 D bends mostly in pipelines which require pigging 40 D bends are used in cross country pipe lines. Thanks and Regards, K.S.Unnikrishnan Kollara On 17-Jan-2022, at 8:09 AM, Engr. Asif Chowdhury <al.istiaque09@gmail.com> wrote: Dear Experts, Hope everyone is doing great. In a cross country gas pipeline project over a bridge deck we have almost completed ou welding activities and right now we are facing problem in selection of Pigs for that pipeline. For your information, the pipeline is about approximately 6 Km in length consisting of  14 nos U-loop and 06 Nos W-loop and 01 nos inlet and 01 nos outlet loops. Outer Dia of Pipeline is about 762 mm with a wall thickness of 25.4 mm. The elbows in the loops are 1.5D 90 Degree LR BW elbows. The entire pipeline has some pipe miter joints included but the angle of miter falls between the range of 2.5 Degree to  5 Degree.   The normal pigs we use for our cross country pipeline having 3D ...

[MW:32752] RE: 32751] Selection of Pigs For 30" Gas Pipeline

Pigging is a very special process. You need to talk to the companies specialized in this discipline. TDW specializes in this area. You may contact them, for specific services in Bangladesh, if they provide so. I know they've a big presence in India. This presentation discusses with some interesting issues, related to pigging . Hope it will help you.   Thanks.   Pradip Goswami.P.Eng, IWE. Independent Consulting Welding & Metallurgical Engineering Specialist Consultant: SNC Lavalin Inc. (Nuclear &Non-Nuclear) Saudi Aramco Approved Designated Project Welding Engineer (DPWR) Qatar Petroleum Approved, SME-Materials & Corrosion Engineering . Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/ Email:pgoswami@rogers.com,pradip.goswami@gmail.com Cell/Whasapp:1-905-9793232   From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Engr. Asif Chowdhury Sent: January 16, 2022 8:55 AM To: Materials & Welding ...

Re: [MW:32750] Regarding weldability and properties of MS and 20MnCr5

Considering new component On Wed, 12 Jan, 2022, 8:50 am 'dwh' via Materials & Welding, < materials-welding@googlegroups.com > wrote: Hello, Is the component part of the front-end assembly of a vehicle? Is it a new component or a worn or damaged part that requires maintenance and repair? Sincerely; 11 1 2022. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/700181e9.c5c49.17e4937ab1d.Webtop.109%40btinternet.com . -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to th...