[MW:26115] NER and Vacuum for cryogenic tank

Good morning every body, Following your knowledge and your experience, please advise me how to determine the nitrogen evaluation rate (NER) for the cryogenic tank. My question: -           Is there any code to control the NER? If no code any procedure or specification on the subject would be appreciated. Also, following the Manufacture's Data Report for the tank, the acceptance standard maximum is 150 mtorr for 72 hours. Is this value (150 mtorr) mentioned in the codes and standard or just manufacturer's standard? Thanks in advance.   -- http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. --- You received this message because you are subscribed to the Google Groups "M...

Re: [MW:26114] Base metals qualified WPQT AWSD1.1

You will get this in section -4 table- 4.2, 4.10, 4.11. Thanks & Regards, Anthony. On Mon, Feb 20, 2017 at 12:15 PM, Umar Rashid Makrani < firoz.makrani@gmail.com > wrote: Hello peers I could not find what is the base metals qualified range as per D1.1  could someone help me, please ? --   With Best Regards, Umar Rashid Makrani, PMP ® ,  AP I653, NACE CIP-2, LEEA Registered Engineer. -- http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com . To post to this group, ...

Re: [MW:26112] About GMAW , metal transfer technique recognition

Arc Voltage less than 21v  is a short circuit/Dip transfer mode THANKS & BEST REGARDS, KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1, CONSULTANT-WELDING & QUALITY Mobile no: +919940739349 On Sun, Feb 19, 2017 at 10:16 PM, Prasad Rode < purode333@gmail.com > wrote: This message is eligible for Automatic Cleanup! ( purode333@gmail.com ) Add cleanup rule | More info Dear sir, All of we know that in GMAW process, there are three metal transfer techniques. 1) spray transfer. 2) globular transfer 3) short circuiting. We know that, as per different temperature, voltage and with different shielding gases also, different technique generated. But, on site and in practicality, how we come to know that welder is using which type of technique. Regards Prasad -- http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm The views expressed/exchnaged in this group are members personel views a...

[MW:26112] Base metals qualified WPQT AWSD1.1

Hello peers I could not find what is the base metals qualified range as per D1.1  could someone help me, please ? --   With Best Regards, Umar Rashid Makrani, PMP ® ,  AP I653, NACE CIP-2, LEEA Registered Engineer. -- http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To post to this group, send email to materials-welding@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJCSKyh3WQFAOsJv28jCtzQVNCLULhK5UzMP%2Bg...

[MW:26111] Re: About GMAW , metal transfer technique recognition

Referring to PQR & PQT, it is defined whether it is spray transfer / globular transfer / short circuiting as per different welding condition(ex., current,) and qualified. In filed, following up one of the three conditions given in WPS which is based on PQR & PQT can target one of the three techniques as you want.  2017년 2월 20일 월요일 오전 8시 40분 13초 UTC+4, Prasad Rode 님의 말: Dear sir, All of we know that in GMAW process, there are three metal transfer techniques. 1) spray transfer. 2) globular transfer 3) short circuiting. We know that, as per different temperature, voltage and with different shielding gases also, different technique generated. But, on site and in practicality, how we come to know that welder is using which type of technique. Regards Prasad -- http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes ...

Re: [MW:26108] welding positionpp

It seems to he 4F. -- http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To post to this group, send email to materials-welding@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b9acb4b6-9d9b-4712-86d4-b548119e5b0a%40googlegroups.com . For more options, visit https://groups.google.com/d/optout .

Re: [MW:26108] PQR for dissimilar material with dissimilar thickness.

See pqr qualification range in sec ix, it guide, u for pqr thickness qualification. -- http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To post to this group, send email to materials-welding@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4f5be64d-1a82-4e09-9cb9-b30d5a398998%40googlegroups.com . For more options, visit https://groups.google.com/d/optout .