Sir,
Not using .because filler,interpass temp.,etc are not same.DSS.
DSS. ER2209
SDSS ER2594
On Mon, 15 Dec 2025, 16:29 Alex Kumar Antony, <alexkantony@gmail.com> wrote:
Can we use Duplex WPS for Super Duplex, kindly quote with the help of codeThanks--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/ee5dcbf4-b6cb-4421-8338-04e109d45b15n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw-Jq4u1udiUYPJrKLrKSktRoFs2z0m_J-r47nrX1Jbq5g%40mail.gmail.com.
Comments