Dear friend,
Nozzle thickness 20.4mm, so your WPS thicknes must be cover 20.4mm. 20mm thick WPS not suitable to use, because 0.4 mm less thick .
Heat treatment is essential variable for WPS. If you use with heat treatment WPS, you have to do heart treatment to job also.
Regards
D.V.Reddy.
On Mon, 15 Dec 2025, 9:14 am Shivasankar A, <shivasankar2593@gmail.com> wrote:
Hi Friends,Refer the attached image,In this, The cover flange thickness is 69.8 mm & The Nozzle thickness is 20.4 mm.the Nozzle is Set on on the Cover Flange with Full penetration Weld the groove is given on the Nozzle pipe.The Final Fillet weld Size is 15 mm.So may i use the WPS which Covers the thickness range from 1.5 to 20 mm?If not, Kindly explain why?Also Tell me the WPS Qualified with Heat treatment can be weld for the Job without Heat Treatment?Looking for your valuable Replies. Kindly Support.regards,A.Shivasankar--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/6032dcdf-efef-437b-b47a-9b89a3fa83e6n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyKn5u98L6GEwm66itbf-z7Fz336jB%2BzzPBStijTcDaG%3DHg%40mail.gmail.com.
Comments