For Valve case it should be from Pouring to final test 
For Plate/Pipe- start from Raw material to final test

On Tue, Oct 8, 2024 at 1:04 PM israr <ahmedisrar.nm@gmail.com> wrote:
Hi 
Can any body respond at what stage an independent inspector witness material testing for certification of 3.2.?


On Wednesday, December 19, 2018 at 6:03:43 PM UTC+5:30 shaikh ahmed wrote:
Dear Friends,

Please can you advise in which EIL Standard or API standard  to find the material certification requirement  EN3.1 or 3.2 or 2.2 for Pumps ( various components) in EIL Specification.

waiting for your response.

thanks.
Ahmed

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f794a65b-0632-4fe1-b9e0-7ed4a33c9c5an%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANgUr0E812Ttxx0vwQtmU%3DyOesxHCEj4_xCXPR%3D_DbN-AMXwww%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...