please guide , what it means to  25 % of which shall be at intersections.

Best Regards,
Abd Ur Rehman
QA/QC Engineer
On Friday, November 8, 2013 at 4:19:23 PM UTC+5 Devang Majithia wrote:

 

Extract taken from API 650. Refer Figure 8.1

 

Regards

Devang Majithia

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Perumal Govindan
Sent: Thursday, November 07, 2013 11:28 PM
To: material...@googlegroups.com
Subject: Re: [MW:19199] RT selection Criteria for API 650 tank

 

Mr. Sam,

Review the MTC of plate material and tolerance of specific heat / lot number and then identify the thickness of the lowest shell course thickness.

 

For lowest shell course, one spot radiography on every vertical joint.

 

Hope this will clarifies your doubt.

 

P Govindan   

On Thu, Nov 7, 2013 at 4:52 AM, Mervin <mervi...@yahoo.com> wrote:

Dear mr sam

 

You can refer the api-650 clause 8.1.2.2 a&b and 8.1.2.3 as mention on this paragraph only spot RT for vertical & horizontal in the 1st 3mter and we use the standard in aramco for intersection joints on top angle to shell.

 

Vin

 



Sent from my iPhone


On Nov 6, 2013, at 9:54 AM, Sam <onlypri...@gmail.com> wrote:

Dear experts,

 

please guide me exactly how many percentage and which area i should select for RT for API 650 tank for below joints.

 

1) shell verticle

2) shell horizontal

3) shell intersections (verticle to horizontal)

4) nozzles

 

i checked API 650 but not getting clear picture hence request to provide standard practice in this regard.

 

regards,

sam.

 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/


 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Legal Disclaimer :  http://mail.gnfc.in/disclaimer

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5b83e661-0620-4813-a52d-b1322a9dd82an%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...