Monday, July 29, 2024

Re: [MW:35145] Buttering

Dear friends,

Anybody have Surveillance sample copy in support fabrications. If anyone have pleas share for supporting me to raise surveillance.

Thanks & Regards,
Sarathi

On Sun, 28 Jul, 2024, 11:34 pm Talha Aamir, <aamirtalha01@gmail.com> wrote:
Hi, 

I hope you are all very well.
I wanted to know the reason behind why we use inconnect and E309L electrodes for buttering? what is the reason behind using those? Suppose a dissimilar weld between low alloy and carbon steel. We do buttering of inconnel on Low alloy metal.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABXHva58aooZKFhCva87G9aSjuKdbvAOH%3DGP_7%2BJb8TnPaHN4Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALFLj9f60DvSm9UXkqdXkUo0NnFWrEcMo%3DSxtG1Ms2kKi5%3D4tQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...