Re: [MW:35143] Buttering

Let us know the production weld condition to respond to your query 
The query can not be answered in isolation 
Is PWHT is applicable ? 
If yes PWHT Parameters?
"Equipment service conditions?
Sent from my iPhone

On 28 Jul 2024, at 11:34 PM, Talha Aamir <aamirtalha01@gmail.com> wrote:


Hi, 

I hope you are all very well.
I wanted to know the reason behind why we use inconnect and E309L electrodes for buttering? what is the reason behind using those? Suppose a dissimilar weld between low alloy and carbon steel. We do buttering of inconnel on Low alloy metal.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABXHva58aooZKFhCva87G9aSjuKdbvAOH%3DGP_7%2BJb8TnPaHN4Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...