Re: [MW:35138] Radiography marking as per ASME Sec. VIII Div. 1

Dear manoj 

       When some part of the vessel undergoes full RT and other part undergoes spot RT satisfying the requirements of UW-11 Asme sec VIII div.1 & where none of the other markings RT1, RT2 & RT3 is applicable then as per UG-116 vessel shall be marked as  "RT4".



Regards
S.Joshi

On Mon, Jul 22, 2024 at 5:25 PM PATEL JAVID <javidpatel89@gmail.com> wrote:
RT4.

On Mon, 22 Jul, 2024, 5:18 pm Manoj Mumbai, <manojacgnr@gmail.com> wrote:
Dears,
Vessel joint efficiency is 0.85
Vessel RT requirement is Spot. 
Dished end having weld seam and fully RTd as the joint efficiency of head is 1 and other parts satisfied as per UW-52 spot RT requirements. So what would be the marking on name plate, RT3 or RT 4 or RT2.
Thanks in advance.
Manoj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5k9Bu4LSKHgJCyfG-Mx33OCokwQRj3%2BpZZ09KwnRQSk7Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANgN0AnN-iabtkHwneX-5i4HR64paYBLq-K6N%2BjddtA5tOdMxw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMMMRBCXBL4A9WBSacOzBA7TRGvKvXN1ut%3D%2BEh16G59UVEFi%2Bg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...