Saturday, July 20, 2024

Re: [MW:35123] Interpass temp

Dear, 

this is specific electrode, E11018M, the manufacturer's recommendations may vary. Typically, the manufacturer's instructions should be followed.

On Sun, 14 Jul 2024 at 4:11 PM, saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear All

    we are used material ASTM A572 Gr 50 and Electrode E11018m for PQR ,
Maximum Interpass how much we can mention in the WPS

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3Omv0KmS7%2B%2B-369L1K%2BOp5OHXZuj-RkTJ_n0_B2GmosZNLw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABJVWh-Wo9L%3Dea-NrgD8BBCWjBb8AUXnQLR7pngpzCkHBbafZA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...