Re: [MW:35112] Procedure Qualification query for Butt and Fillet weld joint

No need ,, procedure test coupon but weld was made means fillet welds also qualified as per sec ix.


On Wed, Jul 10, 2024, 10:54 AM sunil shirke <sunil@spartanindia.com> wrote:
As per ASME sec IX, if welder qualified for butt welding he will qualify for Fillet also. 

Same for Procedure qualification If made welding test coupon by butt joint is it applicable for Fillet Procedure qualification also or not ??

Or need to make different Coupon for Fillet joint procedure qualification. 

Here base material and Filler materials are same for both but and fillet joints

Regards
Sunil 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b1cd034e-68d6-4b4e-9f03-e20a2e820508n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALUa47hWTov512vjjnjDee0pCo8gGBE%3DvX%3DAvjeXFEZ6g85TmQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...