Skip to main content

Re: [MW:35109] Bevel degree in thick plate

Dear All,
Would you be able to explain the difference between SAW and HFW pipe? The client requested SAW Seam Pipe, and that material is not available, so we procured HFW pipe instead of SAW. It can be used. Reference MTC was attached.

Client Pipe specification: 10" PIPE, SEAM SAW, ASME B36.10, BW, TO B16.25, SCH 40, API 5L GRADE B(Ej=0.85
       


Best Regards,
HAFIZ KHAN,
Mechanical Engineer,
KSA.
Mobile No : +966-562887843



On Thu, Jun 13, 2024 at 8:20 PM Amol Betkar <amolbetkar90@gmail.com> wrote:

Dear,

When welding according to an approved Welding Procedure Specification (WPS) for a shell course with a 60-degree bevel fit-up, and then needing to fabricate a thicker shell course, it is crucial to ensure the bevel angle is appropriate for the increased thickness. The following considerations will help determine the appropriate bevel angle for a 130mm thick shell course, assuming materials are ASTM A36 and the design code is API 650:

  1. Standard Bevel Angles: For thicker materials, bevel angles are adjusted to ensure proper penetration and weld quality. While a 60-degree included angle is commonly used for thinner sections like 8mm, thicker sections often require adjustments to the bevel angle to accommodate the increased volume of the weld metal and ensure adequate fusion.

  2. API 650 Recommendations: API 650 does not prescribe specific bevel angles but emphasizes the importance of joint design to ensure quality and structural integrity. Generally, the bevel angle must provide sufficient access for welding and ensure proper fusion.

  3. Typical Bevel Angles for Thick Plates:

    • For plates up to 25mm (1 inch), a typical included angle is 60 degrees.
    • For plates from 25mm to 50mm (1 to 2 inches), the included angle may reduce to around 45-50 degrees.
    • For plates thicker than 50mm, included angles often range between 30 to 45 degrees, with considerations for double-sided welding and multi-pass welding techniques.
  4. Fabrication Practices: For a 130mm thick shell course, it is common to use a compound bevel or a J-groove to reduce the amount of weld metal required and to facilitate better welding conditions.

Given these considerations, an appropriate approach for a 130mm thick shell course with ASTM A36 material under API 650 might include:

  • Single-V Bevel: If using a single V-bevel, an included angle of around 30-45 degrees might be appropriate. This angle allows for deep penetration while managing the volume of weld metal needed.
  • Double-V Bevel: For very thick plates, a double-V bevel could be used to balance the welding from both sides, typically with each side having an included angle of around 30 degrees.

Recommendation: For a 130mm thick shell course, a 30 to 45-degree bevel angle should be appropriate. A double-V bevel (each side 30 degrees) might also be considered for such thickness to ensure welding quality and manage distortion.

Always ensure that any change in bevel angle or welding parameters is reflected in an updated WPS, approved by the relevant authority or quality assurance team, to maintain compliance with API 650 and ensure structural integrity.

AB


On Thu, 13 Jun 2024 at 15:53, Mashood Khan <mashood@epic.com.pk> wrote:
Concern is to confirm that i am welding as per approved WPS 8 mm Shell course with 60 degree bevel fit-up both sides,  and if i fabricate 130mm thick shell course weld what should be  the appropriate bevel degree (As i don't have WPS now in my hand).
Materials are M.S. A36 for both tanks.
 Designing Code is API 650

Regards,
Mashood Ahmed Khan
EPIC Pvt. Ltd.
P:034627949880309-8885421
 "The man who best understands time is he who is not taken aback by its proceedings." 
 (Ali Ibn Abi Talib)


Mailsuite Sent with Mailsuite  Ā·  Unsubscribe
06/13/24, 11:00:28 AM

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD3cn5jJfMv5H1ybKq_G%3DnuBYH1X5FM4Nmg-or1eBEy9%2BvccAw%40mail.gmail.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1o3gCA_oykoYa3W_ssKpE16FC0QsaO0Z-9UsWWOrUZ7jg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMq6b79QW%3DMiXYzOggqNAkRmAcgEVCOtf4cj1%2B9SQB-%2B_SG9VA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...