Re: [MW:35097] Welding of SS on CS

You have to use SS309 filler metal in order to get austenitic weld metal of the joint. SS316L filler metal will provide you martensitic weld metal due to dilution with CS.

On Tue, Jul 2, 2024 at 6:28 AM Talha Aamir <aamirtalha01@gmail.com> wrote:
Why cannot weld SS 316L on CS directly? Why do we need to use the SS 309 welding rod on CS to provide a base to weld SS 316L?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABXHva65M9GtbE6y2Li-YBHMGyowfeTFyzmKrt%2BGN%2BBaKL3XeA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BENTMKp5hf%2BE3oBgt8VBHpCyruEoZgkLOQ9vBGZmPUi-vgaUQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...