Monday, July 29, 2024

[MW:35147] RELATED WPS AND FILLER WIRE

Hii Expert,

I have WPS SMAW + GTAW (5.5  MM THK.-DEPOSITED 11 MM THK)-MATERIAL ASTM 106 GRB , CAN USE SAME WPS IN FULL GTAW WELDING METAL THK. IS 7 MM..


And I have C-1020 material which filler wire & Electrode  can use in full GTAW PROCESS and SMAW PROCESS


THANKS

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/82ee3a09-1b4b-4e77-bb92-eaeb9faee693n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...