            Can I combine  the  following  PQR ?,if  yes  then what will base  metal  thickness  range   or is it require  to mention separate  qualification  of  dissimilar  thickness?

PQR  36  : 
       Base metal  : P.No. 1 Gr 1 to  P.No.1 Gr  2 
       Thickness    : 32 mm to 5.5 
       Process :  GTAW + SMAW 
       Testing : Tensile ,bend ,Impact @ minus 46
PQR 36 A : (additional  PQR only impact tested )
       Base metal  : P.No. 1 Gr 1 to  P.No.1 Gr  2 
       Thickness    : 32 mm to 5.5 
       Process :  GTAW + SMAW 
       Testing : Impact  @ minus 56 
PQR 29 :
       Base metal  : P.No. 1 Gr 1 to  P.No.1 Gr  2 
       Thickness    : 6 TO 6 mm 
       Process :  GTAW + SMAW 
       Testing : Impact  @ minus 46

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/97654a25-1eae-4cdb-943e-419391048c43n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...