Monday, July 29, 2024

[MW:35140] comment recive dfrom client

Dear Sir
i have recived a comment from my customer on PQR submitted as our PQR/WPS code edition 2015 is PQR dated 07.02.2019 what is the format or document to show it was used in last year ,we are using same since last 5 year.

 "'It is not allowed to use PQR issued five years before their application for the equipment construction unless VENDOR can demonstrate that the relevant WPS has been used during the last 5 years. The WPQR shall contain a document, which assure the welder activity shall be according to adopted Code"".

Kindly let me know what reply, and pls send me format of  Weld plan, weld map and test plan

Regards

asif Mulla

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/93693dd8-bc8d-4833-b1b3-d3192329642fn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...