Re: [MW:34799] SS 310 TO SS 316 & SS316 TO SS304 Welding joint qualification & filler wire

Find attached the following answers: 

1)Can we weld SS310 TO SS316 with the above pqr and what will be the filler for the same? 

No, you have to requalify the PQR as A No. Change from 8 to 9. 
Filler: SS310

2)Can we weld SS316 TO SS304 with the above pqr and what will be the filler for the same?

Yes, if Impact is not applicable. 

On Sat, Mar 2, 2024, 14:57 Soumen Samanta <ssoumen05@gmail.com> wrote:
Dear Expert,

We have PQR base metal SS304 TO SS304 & filler wire ER 308L 
I have the following question 
1)Can we weld SS310 TO SS316 with the above pqr and what will be the filler for the same?
2)Can we weld SS316 TO SS304 with the above pqr and what will be the filler for the same?


Thanks in advance

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/33355d65-cf1b-48c3-bab5-3c223407725an%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zf9nULZOfjCjUhh8VcA-jX9Atje4vjCeO8P%2BFPSw8B54w%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...