Friday, March 29, 2024

[MW:34833] arcap and 306L welding

Hello everyone,

I want to weld ArCap material and 306L material together. But I have some problem. I can't achieve a leak-proof seal.

I use laser welding. And The thickness of the 306L material is very low that is 0.6 mm. What should I use as welding wire? I couldn't find it. Or do you have any other suggestions.

Thank you

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/78f24dcb-67cb-420f-a040-7cde2fcd561cn%40googlegroups.com.