[MW:34785] clarification require for WPS & PQR qualification with impact test


dear expert
we have to do qualification wps ,pqr for the below mentioned materials as per ASME section 9.

Test coupon
SA 516 Gr 70 (P-1 G-2) -Thickness 20 mm
with
IS 2062 E 350 C (Unassigned Metal) - Thickness 50 mm
Code - ASME 
Position - 3G
Process - SMAW 
Electrode - E-7018
Impact =  -20C @ 27J

Question
1) what is the minimum & maximum thickness qualified with impact?(code reference).
2) what has to be considered during and after impact results?(comparing with base metals)
3) Whether Thickness "t" weld metal deposit in coupon should be 13 mm or 3 layer minimum in single side to qualify for maximum to be welded ? 

Thanks in advance.Do the needful. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOp_kKgYrfxS7%2B7LOv5Ow4R%2B1d8WVXgURzsy_NMJZ26nobS9kg%40mail.gmail.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...