On Thu, Feb 29, 2024 at 1:49 PM Ajay Paul <ajaykp995@gmail.com> wrote:
Dear Experts ,i need some clarificationi need 50mm thickness blind for hydrotest,but i dont have that thickness so can i use welded 30mm+20mm blinds for it?Pls. suggest .--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b9e91e1e-4210-44a7-a40a-0cf05d968854n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0wW4gufvS9OXWQR_uWnANqkcQAjMCQwAUN0%3DAvtvHQosQ%40mail.gmail.com.
Comments