Saturday, March 23, 2024

[MW:34825] Inquiry about Single Bevel with Back Grinding

 Dear all , 

I am writing to seek clarification regarding the classification of single bevel with back grinding in terms of whether it is considered as with backing or without backing.

 Could you please provide information or guidance on this matter? Any insights or references you can share would be greatly appreciated. 

 Thank you for your attention to this inquiry. I look forward to hearing from you soon.


 Best regards, 

   


Masna Uday Kumar

masnaudayk4@gmail.com

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOOs2YZu42Lu509ky9oEa9rqxOV6o1SdX6E4eHLWyV8ha3Xc1A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...