Dear Experts

In the bent 3/4 "pipe that I have specified below, my customer tells me that I need to do a procedure and test on how much thinning I have done by my customer. Accordingly, Asme Sec. VIII, which tests and which standard should I refer to in order to see how much thinning I have done in the project I have done according to the standard?

resim_2024-03-07_084909277.png
Sezgin .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3c33923b-aca8-422d-8dda-249359bfe41cn%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...