Re: [MW:34791] Blind thickness for hydrotest

Dear Team,

Please find the attached Plate made Blind Chart for easy reference.

Regards
G Mohanraj

On Fri, Mar 1, 2024 at 2:03 PM Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:

thickness calculation for temporary blanks as per code B31.3  for your reference.

 



On Thu, Feb 29, 2024 at 1:49 PM Ajay Paul <ajaykp995@gmail.com> wrote:
Dear Experts ,
        i need some clarification 
i need 50mm thickness blind for hydrotest,but i dont have that thickness so can i use welded  30mm+20mm blinds for it?
Pls. suggest .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b9e91e1e-4210-44a7-a40a-0cf05d968854n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0wW4gufvS9OXWQR_uWnANqkcQAjMCQwAUN0%3DAvtvHQosQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEkUWtKAYSR-LCmPAVQ1DpqnqSkqiTRA_2vjvA5Xx50EXdxr9A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...