Re: [MW:34778] WPS & PQR for P8-P1 and P8-P8 as per ASME Sec.IX

Dear Sanjay

Yes you can use, but subject to : 
1. No Charpy Impact Test requirements 
2. No Heat Treatment requirements

Thanks 


On Thu, Feb 29, 2024, 16:10 SANJAY SINGH <sanjay.kharwar349@gmail.com> wrote:
Dear Experts ,
            Can anyone suggest my below queries
1. I have WPS and PQR with P8 to P1 Base metal  Grade 316 to E250 BR then can I use this PQR for SS304 Grade base metal welding .
2. Similarly I have P8-P8 WPS , PQR in Grade SS316 then can I use this PQR for the welding of SS304 base metal.

Pls. suggest .

Regards 
S.R.Singh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALkBf%2Bvy_kF3j1y74J5pGKcVhMfvCaeEUk%2BCNA8hUd%2B9-Lab%3Dg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zeOyX%2BKNaOqPwfD4B-bc_VdSfkPQ0Nmys0fvF4g1hksQw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...