Re: [MW:34774] P-No. of UNS 06626

Dear all,

Please refer to the table below for the required chemical composition of UNS 06626 under case 2276, as per the ASME BPV code cases. The P-No. for material UNS 06626 is P-43.



On Wed, Feb 28, 2024 at 11:57 AM cyndiso yapi <cyndsp9@gmail.com> wrote:
Its P-No 43 check ASME IX Table QW422 it's listed there 

On Wed, Feb 28, 2024 at 12:12 PM ilham fauzi <ifilham@gmail.com> wrote:
Dear Experts,

What is P-No. of UNS 06626, my client say its P No.45 but that materials simillar with UNS 06625 which is its P-No.43. Please for the advice

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c105a43f-72c7-44b6-96e1-0e11095552a3n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABktmDfFasCLFOTjL_7%2Bogw_AjzR2T_aTCeoV_oOr%3DZTNiH7kw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zYAakAwiLyp2J3AqpDMTSFAhCZXPSKUY5ZFFYy2gTh8Q%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...