On Tue, 27 Feb 2024 at 17:43, 'SENTHILKUMAR SWAMINATHAN' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hello Dears,

Please give you input when PQR for Piping done - Client spec is silent in NDT Acceptance criteria. Which code Acceptance criteria should use for NDT?

ASME B31.3 or ASME IX.

Thank you, 
Regards, 
S.SENTHILKUMAR

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/750277828.828737.1709031941988%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OifUeObQGgsYQ6WE0dSx7v2%3DB6kuBH5TQUDPUECyNijAA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...