Sunday, February 25, 2024

Re: [MW:34761] Re: FILLER WIRE

If you want to use different welding process , ER70S & ET70-1,,But need SMAW then you want to conform your parent material tensile strength based on this you can select 6018 or 8018 ......etc

On Fri, Feb 23, 2024 at 11:11 AM Mohd Siraj <mohd52100@gmail.com> wrote:
AWS A5.1 E7018 or equivalent.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5f8647ae-934e-4e2f-9f75-1adaa7e56857n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEE6Dzco6%3DQJv-BPrgYx12Gu16e%3D81TLxVG%2BsiWAeEu8hLQjgg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...