Re: [MW:34760] Re: A 333 Gr.6 toughness test

hi 
If SA333 LTA materials it already qualified in -46 Dec just you want to conform  impact test it passed. then -10 Deg no issues ....
and same if you want to save materials cost use SA 106 Gr. B  also  you want to test impact temperature -10 Deg.....

regards
RK

On Sun, Feb 25, 2024 at 6:55 AM rohit barge <bargerohit96@gmail.com> wrote:
No issue because it is come with impact tested to -45 Deg and your temp is -10 Deg you just tell your client give them code reference as this grade can use upto -45Deg so you can use it no issue in that.

Thanks & Regards

Mr. Rohit Barge

   

On Fri, 23 Feb 2024, 1:41 pm Mohd Siraj, <mohd52100@gmail.com> wrote:
no, replace the pipe.

On Saturday, December 30, 2023 at 2:40:52 PM UTC+3 dia shukr wrote:
Hi friends

I have pipe A333 Gr,6 with design minimum temperature (-10C).Will I need to do a toughness test??As you know, depending on table A-1 in ASME B31.3 the minimum temperature is (-50C).

Thanks every one

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/87aef01c-241f-4484-a4ea-7422abf8fb47n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHK93nLBQfZ_w05Ubu_%2B7h4ztEiD3_3Gybv40S_H4KRdsKXvsg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEE6DzcZbuPk4mQ4KHLUEig-HOqUUb7q48YwZFkbtF9f_5HozA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...