would you pl provide, fluid service and service temperature., this can be happened due to any sudden/abrupt changes in process or parameter.



On Monday, December 25, 2023 at 1:54:15 PM UTC+3 Manish Kumar wrote:
Hi,
As per attachment please share the information about damage mechanism and mitigate action to prevent the ice formation in SS316 material.


Regards
Manish Kumar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cb6d211c-eb68-4259-9731-bad675f69434n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...