Wednesday, July 26, 2023

Re: [MW:34447] GAUGE LENGTH REQUIRED SA105 MATERIAL

Please refer ASTM A370 or ASME SA-370.

Please also refer ASTM E8M section 6.10

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, 26 July, 2023 at 01:55:09 pm IST, Sam <samraja224@gmail.com> wrote:


Dear Expert,

Gauge length shall be reported in MTC as per ASME SA-105 material. 

Kindly confirm and reference clause.


Thanks,
Sam-Kuwait

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6ce53999-6582-47f4-9399-ae6e7d9da8fdn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...