Wednesday, July 26, 2023

Re: [MW:34444] Clarification regarding T,K,Y JOINTS WELDING

As per AWS D1.1, 6GR is required

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Jul 26, 2023 at 1:18 PM Uma sankar Sankar <umasankar6246@gmail.com> wrote:
Dear Experts
                        Can 6G qualified welder can weld T,K,Y joints,yes or no.If yes why,if no why.
Why only 6GR qualified welder only can weld T K Y JOINTS?
What type of NDT required?
How to weekly Repair rate of welder.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO8WSnGALirhW4vroU5hACX-VMQLLvxm4FrmX5dEfEMYb1v45g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePc6Se%2Bc25T87wpjYRGOmiYZygFiu%2BHpovc0NUH01rkmw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...