Re: [MW:34374] REGARDING ISSUE IN MONEL 400 TUBE TO TUBESHEET JOINT WELDING

Welder skill is very important, Too much current,
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Tue, Jul 4, 2023 at 10:07 AM Saurabh Joshi <saurabh.joz30@gmail.com> wrote:
Dear All, 


       We are facing cracking  of tube ends , dis-bonding between tube base material and filler material during welding in Monel 400 Tube to Tubesheet Joints. Refer attached photographs.
Tube MOC: SB-163 UNS-N04400; 25.0 mm OD x 2.0 mm thk
Tube sheet MOC: SA-336M Gr F304L + SB-127 UNS-N04400 (48 + 10 mm thick clad by Explosion Bonding)
Welding: ERNiCu-7 GTAW filler size 2.0mm  with Argon shielding gas.


Kindly share the reason for such cracking, disbonding  and Suggest Corrective and preventive actions regarding this issue.

Thanks in Advance.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/70d8c114-8503-4ad0-b5db-22db6d57871en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOsyeLjqoaZ%2BWZDm4ketUPigS4iJz1T36w%2BLbSUH6iMDw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...