ASTM A 692 pipe joint welded on June 10th 2023 ,NDT RT result was failed , while attending  repair,come to know that drawing revised on June 20th ,As per revised drawing required pwht.As per old drawing pwht not required.
What may be the root cause?
What will be the proposed correction?
If the pqr done with pwht ,is it possible to prepare wps with and without pwht?

But pwht is Essential variable for welding procedure specifications?
During investigation 15 joints were found in the same situation, what will be the action can we take?
I believe,I will get the best answer 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO8WSnHu%2BQYskt45fD%3D0OLu191z5ZeFGERTWLuvVx_qofTmkZg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...