Wednesday, July 26, 2023

[MW:34440] Impact test requirement for Reinforcing pad plate for Non Sour Service

Hi team,

Kindly advice the requirement of impact test for Reinforcing pad plate which is welded to the main header. Kindly note that the main header pipe is already impact tested.

Service: Non Sour
Lateral Material: SS316/316L
Lateral Sizes: 
60" X 30" 
60" X 42" and 
60" X 52"
Code: ASME B31.3

Thanks in advance.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3e26c23c-8746-4e43-ac3a-14acc0ff8354n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...