[MW:34435] selecting Proper storage tank material - Advise

Dear Gents,

Kindly support selecting the proper storage tank material of Sodium Polycarboxylate.
currently, I have 100 ton CS storage tank of  Sodium Polycarboxylate the internal Stainless steel 304 cladding 2mm sheets.
After one year of operation, we found corrosion spots and  Sodium Polycarboxylate leakages.
internal SS 304 cladding welding joints by Argon welding - 7018 welding wires.
tank tested by water and it was excellent without any leakages.
The  Sodium Polycarboxylate data sheet is attached.
I've attached photos of the corrosion.

Please advise which material I should select to fabricate a storage tank for  Sodium Polycarboxylate and how to solve current corrosion spots.

thanks. 

ploy 1.jpg

poly 2.jpg
poly 4.jpg
poly 5.jpg

poly 6.jpg

0c7f1879-b709-4cb5-846d-617afb87ba3e.jpeg



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/90877f70-4bd6-4e6a-8e96-ff5be76b65c3n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...