Thursday, July 20, 2023

[MW:34433] Attachment unknown material to pressure part welding UG-4(b)

Dear Expert,

Attachment clip material is Unknown (As per drg SA240 TY SS304L) to pressure part is shell (SA516 GR.70N). No MTC and traceability for attachment material. Same to be used in 'R'-Stamp repairing vessel.UG-4(b).JPG

Cases,
1, Can weld with PMI and Hardness testing of unknown and verifying weldability and strength of replacement material as per sec viii-1 and NBIC ?
2, Can use No traceability (No product marking) material as per ASME SEC VIII-1 for attachment welds ?
3, Can use SA240 TY316L with traceability material instead of SA240 TY304L (different grade)?

Kindly advise us.

Sam-Kuwait

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/420389aa-462a-49c3-b477-e003a24bd7ecn%40googlegroups.com.

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...