Monday, July 10, 2023

[MW:34397] Re:


As per ASME Sec-IX, If you want to use the Root Pass of one PQR on second PQR, it should be qualified on at least 13mm thick coupon.
Hope this will clarify.

Capture.PNG
On Monday, 10 July 2023 at 06:11:27 UTC+3 Srinivas Rao wrote:
No , not allowed , you cannot make any WPS more than the thickness of maximum allowed range of Each PQR.
at least one PQR should have been qualified to support maximum thickness of you required to prepare WPS.

Thanks & Regards,
Srinuvasarao 
welding Engineer 
On Monday, June 19, 2023 at 7:47:05 AM UTC+4 Soumen Samantha wrote:
In my opinion you can not weld 25 mm thk.

On Sunday, June 18, 2023 at 9:40:34 AM UTC+5:30 sujit kumar wrote:
Dear all,

I am having material thickness SS316   25 mm to weld.
1.  i have qualified  GTAW PROCESS WPS with  10mm plate which is allow 2T up to 20 mm  thk weld 
2. another i have qualified SMAW with back chip WPS with 10 mm Plate which is allow up to  20 mm SMAW only with Back chip.

may i allow to do 25 mm thick welding with Both  gtaw +smaw  welding.




sujit

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/be9bc4db-6bb7-487e-818e-4f9de2acec6an%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...