[MW:34377] Re: 316Ti material - GTAW rod selection

ER318 is a compatible filler metal 

Thanks

Vishwas - IWE 
International Welding Engineer


On Wednesday, July 5, 2023 at 12:04:28 PM UTC+5:30 PARAI Reaction Channel wrote:
Dear Sirs,

Please guide for the selection of GTAW welding rod to weld SS 316Ti pipe shell.

Can we use ER318, as I searched in Google?

Please  confirm and also advise for any special wedding parameters,  shield and purge gas requirements for this welding. 

Regards, 
Saravanan Sornam, 
ANSAN city,
S. KOREA. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dda38699-f496-4709-a5d9-f48fac46ca11n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...