Re: [MW:33884] Low alloy vs high alloy steel

Low alloy less than 5% of individual or aggregate of total number of alloying elements ,  greater  than 5% and less than 10.5% is medium, and above 10.5 high alloy as mentioned for low alloy.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Dec 28, 2022 at 11:53 AM mithlesh kumar <mithleshmech47@gmail.com> wrote:
Dear expert ,

Please brief difference between low alloy steel vs high alloy steel.

A335 P9 is low or high alloy steel.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/62edc733-0051-4b57-9c08-171a8ff85d71n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOrc4TROqYtGpA3uCEGnW7pdivuzYrbSMEUWKorOMO3eQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...