Monday, December 26, 2022

[MW:33861] Welding Cast Iron & G.I

Dear Experts,

Does any one experienced welding of G.I and Cast Iron in their career time, Is it possible to weld the said metal, if someone has the experience please share the details of the same.
As we are trying to weld the said metal  it is cracking at the same time before cooling.


Your comments will be highly appreciable.

Thanks & Regards,

Manoj Singh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPkJdRKuv05CRTxrUAWWNR%2Bh_QG0zpmgucnxbc50imwgBW9O1Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...