[MW:33826] Re: Vanadium composition showing in p91

Kindly read WP22 instead of P91
On Saturday, December 17, 2022 at 8:15:23 PM UTC+5:30 mithlesh kumar wrote:
Dear team,

I have observed vanadium in heat analysis of p91 MTC  , but as per code vanadium is not showing in chemical composition table. Suggest is it acceptable or not if acceptable code reference please.

--