you can extract sample, 1.5mm from bottom that for root process and one from middle that from smaw. --
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/00b3c3b1-2607-416a-a2e9-5d9b8d666287n%40googlegroups.com.
so if u refer figure for impact it is quite clear.
however meaning is same u stated.
On Thursday, December 15, 2022 at 7:06:37 AM UTC+3 fernando...@gmail.com wrote:
referring to impact tests for qualification of welding procedures, it is reasonable to define that for the design situation according to ASME B31.3, in circumferential joints welded by two processes (GTAW -root / SMAW - others), each process must be separately impact tested (in the same way as it is done today for ASME VIII div 1)?There is no text that makes this statement explicitly on B31.3.Thanks and regards,Fernando Lescovar Neto IWE
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/00b3c3b1-2607-416a-a2e9-5d9b8d666287n%40googlegroups.com.
Comments