its is acceptable as per asme spec .

On Sat, 17 Dec 2022 at 20:15, mithlesh kumar <mithleshmech47@gmail.com> wrote:

Dear expert 

Today i have reviewed one MTC of WP22 and found that vanadium is given in heat analysis inly but as per code chemical table it's not required isnit acceptable or not if acceptable code reference please.
Thanks 

On Saturday, July 30, 2022 at 7:30:30 PM UTC+5:30 gmvs...@gmail.com wrote:
Dear Mithleash 

To avoid conflicts Need to discuss the same with client if needed up to end user for acceptance, 

All the parties should agreed for the test to be conducted, and its acceptance limits, since some time client specification has some stringent requirements, 

Regards

Sathiyanarayanan

7358752505



On Tue, 26 Jul, 2022, 10:22 am mithlesh kumar, <mithles...@gmail.com> wrote:
Dear Expert,

we have some pipes of 316 material all pipes are off cut and heat identification is not available on these pipes. MTC type requirement is 3.2 also we have not MTC. what is the Procedure to certify the material as per the 3.2 type requirement? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c083e4ed-c02a-49dc-b2a4-c3d8c8c8c738n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4a0d8eeb-4211-4390-92ad-8b2e0530bb31n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k-Zv1PdhOZ4hKh2id%3DJvxVR8W77eFPkZ-EHEBx40xYAvA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...